Statuario
Highlights:
FIRE REACTION (EUROCLASSES) | EUROCLASSES UNE-EN-ISO 9239-1:2002 & ISO 1716:2002 | Euroclassses | A2fl s1 |
LINEAR THERMAL EXPANSION COEFFICIENT | UNE EN 14617-11:2006 Agglomerated stone. Determination of linear thermal expansion coefficient. | ºC-1 | 2,06 x 105 |
FLEXURAL STRENGTH | UNE EN 14617-2:2005 Agglomerated stone. Determination of flexural strength. | MPa | 45 – 55 |
IMPACT RESISTANCE | UNE EN 14617-9:2005 Agglomerated stone. Determination of impact resistance. | J | 8 – 11 |
SLIP RESISTANCE | UNE EN 14231:2004 Tiles of natural stone for external paving. Requirements and test methods. | USRV | 6 wet 37 dry |
WATER ABSORPTION | UNE EN 14617-1:2005 Agglomerated stone. Determination of water absorption. | % | 0,06 – 0,08 |
APPARENT DENSITY | UNE EN 14617-1:2005 Agglomerated stone. Determination of water absorption. | kg/m3 | 2,350 – 2,450 |
ABRASION RESISTANCE | UNE-EN 14617-3:2005 Agglomerated stone. Determination of the abrasion resistance. | mm | 26 – 28 |
CHEMICAL RESISTANCE | UNE EN 14617-10: 2005 Agglomerated stone. Determination of the chemical resistance. | C4 | C4 Alkalis: Materials maintaining at least 80% of their resistance reference value after 8 hours. Surface hardness |
SURFACE HARDNESS | UNI EN 101 Ceramic tiles. Determination of scratch hardness of surface according to MOHS. | MOHS | 6 -7 |
Statuario Altissimo
Highlights:
Centimeters / Inches | Thickness | Lucidato Shiny | Soft |
---|---|---|---|
270x120cm | 6mm | UM6L27012441 | UM6S27012441 |
120x120cm | 6mm | UM6L120441 | UM6S120441 |
Venatino
Highlights:
FIRE REACTION (EUROCLASSES) UNE-EN-ISO 9239-1:2002 & ISO 1716:2002 | Euroclassses | A2fl s1 |
THERMAL EXPANSION COEFFICIENT UNE EN 14617-11:2006 | ºC-1 | 3,3 x 105 |
FLEXURAL RESISTANCE UNE EN 14617-2:2005 | MPa | 80 – 90 |
IMPACT RESISTANCE UNE EN 14617-9:2005 | J | >15 |
SLIP RESISTANCE UNE EN 14231:2004 | USRV | 6 wet 37 dry |
WATER ABSORPTION UNE EN 14617-1:2005 | % | 0,06 – 0,08 |
APPARENT DENSITY UNE EN 14617-1:2005 | kg/m3 | 2,060 – 2080 |
ABRASION RESISTANCE UNE-EN 14617-3:2005 | mm | 28 – 30 |
CHEMICAL RESISTANCE UNE EN 14617-10: 2005 | C4 | C4 Alkalis: Materials maintaining at least 80% of their resistance reference value after 8 hours. Surface hardness |